Songshun Steel & TOP Steel Manufacturer Supplier in China

XPM Injection Mold Material Cold Rolling Process Always Encounters Pitfalls?

DIN XPM ESR steel is a high-performance, high-purity plastic mold steel from the German Gröditz tool steel series. Renowned for its exceptional polishability, uniform hardness, superior thermal conductivity, and high wear resistance, it is highly favored in the field of high-end mold manufacturing. However, the cold rolling process, which is crucial for imparting enhanced performance to XPM injection mold material, often presents numerous challenging issues for many manufacturers. These problems can lead to compromised material properties, reduced production efficiency, and even impact the final quality and service life of the molds. Drawing on our extensive production experience, Songshun will analyze the core challenges encountered during the cold rolling of this material and provide targeted solutions, committed to delivering the optimal materials to customers worldwide.

I. Surface Cracks

1.1 Problem:

XPM cold rolling cracks (edge cracks, longitudinal cracks, transverse cracks, crazing, network cracks, etc.). In severe cases, they propagate along the rolling direction. These cracks are magnified during subsequent processing, leading to direct scrappage.

1.2 Cause Analysis:

(1) Excessive deformation: The formation rate of shear bands inside the material exceeds the critical value. An overly large single-pass reduction causes localized internal stress concentration.

(2) Lubrication failure or improper application.

(3) Temperature control loss: Local excessive temperature rise or uneven cooling during cold rolling increases the phase transformation stress of the material structure.

(4) Insufficient annealing prior to cold rolling, leaving residual stresses unreleased.

(5) Uneven carbide distribution or impurity segregation in the material, triggering the propagation of micro-cracks during cold rolling deformation.

1.3 Solutions:

(1) Strictly control the single-pass reduction rate. It is recommended to adopt a “multi-pass, small deformation” cold rolling strategy instead of blindly pursuing efficiency.

(2) Upgrade the lubrication system by adopting extreme pressure anti-wear rolling oil to establish a stable lubricating film and reduce the friction coefficient.

(3) Implement an infrared temperature control device to monitor the temperature of the rolling zone in real time, controlling the fluctuation range within ±5°C.

(4) Optimize the pre-cold-rolling annealing process to ensure the XPM material has sufficient plastic reserve, which is a prerequisite for successful cold rolling.

(5) Select high-quality XPM billets to improve material purity and ensure uniform carbide distribution. Improve production through powder metallurgy to avoid component segregation issues inherent in traditional casting.

II. Surface Quality Defects

2.1 Problem:

Surface defects such as roll marks, pits, scratches, bubbles, scale, or pitting occur on XPM injection mold material. These defects severely compromise its polishability and subsequent chrome plating process, potentially leading to “pinholes” or “orange peel” defects after polishing, resulting in poor finished product appearance.

2.2 Cause Analysis:

(1) Deterioration of roll surface condition, including contamination, severe wear, or coating spalling. Furthermore, the hard carbides in XPM steel accelerate work roll surface wear during cold rolling. The spalled particles adhere to the rolls, causing “roll sticking,” which leaves periodic indentations on the strip surface.

(2) Poor process lubrication, and incomplete removal of scale and oil contamination from the raw material surface before cold rolling, which then enter the rolling process, causing residues or pits.

(3) Improper coordination between pickling and rolling processes. If the mill scale on the surface of the hot-rolled XPM base material is not completely removed, it will be pressed into the matrix during cold rolling, forming pitting and oxide spots. Inadequate drying after pickling results in acid stains.

2.3 Solutions:

(1) Implement roll texturing and a regular roll change system. Additionally, perform routine roll polishing, cleaning, and inspection. Replace rolls promptly upon detecting pitting or chipping to prevent surface defects from being magnified exponentially.

(2) Adopt specialized cold rolling oil containing extreme pressure additives and neutral water-soluble lubricants to ensure uniform lubrication covering the entire rolling surface and reduce friction.

(3) Add pickling and cleaning processes before cold rolling. Thorough pickling and descaling are mandatory, utilizing a “two-stage pickling + high-pressure water washing” process to completely remove scale and oil contamination from the raw material surface. Strengthen quality control of the pickling process by adopting a combined “high-efficiency hydrochloric acid pickling + neutral salt electrolysis” process and adding a hot-air drying section. An online surface inspection system can also be introduced for real-time monitoring of material cleanliness.

Timely drying after pickling to prevent secondary rusting; conduct strict incoming material inspection to reject raw materials with surface scratches or pits, avoiding defects at the source.

(4)Utilize advanced heat treatment and surface treatment technologies to improve surface smoothness and thereby reduce the defect rate.

III. Dimensional Deviation

3.1 Problem:

XPM injection mold materials demand extremely high dimensional accuracy. However, this steel exhibits significant dimensional fluctuations after cold rolling, making it difficult to ensure product consistency.

3.2 Cause Analysis:

(1) Unreasonable process parameter settings, with an imbalance in reduction, rolling speed, and tension control, leading to excessive cumulative dimensional deviation.

(2) Unrelieved internal stress. As a pre-hardened steel, DIN XPM inherently contains residual stress. If not subjected to annealing softening prior to cold rolling, the residual stress is released during the rolling process, causing uneven deformation, dimensional deviation, and poor flatness.

(3) Inhomogeneous microstructure during the smelting or casting of DIN XPM mold steel, such as inconsistent grain size and varying phase compositions, can lead to dimensional instability after cold rolling. Additionally, the thermal conductivity of XPM tool steel is 20% higher than that of conventional mold steels. Local overheating during cold rolling causes thermal expansion, resulting in dimensional deviation.

3.3 Solutions:

(1) Optimize process parameters for precise control. Develop a multi-stage rolling schedule based on the thickness and hardness of the XPM mold material. After each pass, promptly inspect the thickness and flatness, and fine-tune the parameters for the next pass based on the results to ensure cumulative deviations remain within tolerance. Utilize finite element analysis (FEA) to simulate the mechanical behavior during cold rolling, optimizing parameter settings to enhance dimensional accuracy control.

(2) Select XPM material pre-hardened to an appropriate hardness level to reduce cold working deformation and improve microstructural stability.

(3) Optimize the material microstructure through controlled smelting and casting processes to ensure uniformity, minimizing issues such as grain size variation and phase composition differences. Monitor the temperature in real-time during cold rolling and use XPM raw materials that meet purity standards.

IV. Excessive Work Hardening

4.1 Problem:

After cold rolling, XPM injection mold material exhibits an abnormal increase in hardness and a decrease in ductility, leading to difficulties in subsequent machining and even “brittle fracture”.

4.2 Cause Analysis:

(1) Cold deformation causes a sharp increase in dislocation density within the material, resulting in severe work hardening.

(2) Grains are elongated and a large number of substructures are formed, increasing material strength but reducing ductility and machinability

(3) Cold working induces the transformation of retained austenite to martensite, further increasing hardness.

4.3 Solutions:

(1) Implement an intermediate annealing process to restore cold rolling formability.

(2) Perform low-temperature tempering after cold rolling to improve machinability while maintaining strength.

(3) Enhance microstructural uniformity and machinability through vacuum degassing treatment.

Conclusion

In the cold rolling process of XPM injection mold material, in addition to the core issues discussed above, other potential challenges may also arise. Therefore, strict control is required across multiple dimensions, including material selection, process optimization, and personnel operation, to provide effective solutions. At Songshun, we rigorously oversee every critical detail in the cold rolling process of XPM injection mold steel, and are committed to providing robust material support for the development of the industry.

Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways