Songshun Steel & TOP Steel Manufacturer Supplier in China

What Challenges Are Encountered in the Hot Rolling Process of DIN XPM Die Steel Plate?

The hot rolling process endows XPM steel plates with their final mechanical properties and service life, granting them superior polishability, uniform hardness, wear resistance and other advantageous characteristics, which makes the material widely applied in various fields. However, any slight negligence in the hot rolling of DIN XPM die steel plate will lead to various defects and technical challenges, all of which require prompt resolution. This paper will conduct an in-depth analysis of the core problems, their causes and corresponding solutions in the hot rolling process.

Common Problems and Solutions in the Hot Rolling Process of XPM Die Steel Plate

1. Surface Oxidation and Crack Defects

  • 1.1 Problem: During the hot rolling of DIN XPM die steel plate, scale, local longitudinal cracks or edge cracks occur on the surface. These are the most common and highly detrimental defects, which not only increase the subsequent processing costs, impair the appearance but also deteriorate the mechanical properties, and even lead to scrapping of the products.
  • 1.2 Cause Analysis:
    (1) Under high-temperature conditions, the surface of the steel plate reacts with oxygen in the air to form an iron oxide layer.
    (2) Impurities on the raw material surface (e.g., oil stains, rust) are not completely removed, and a large amount of gas is generated during heating, forming a porous oxide layer.
    (3) The billet itself has inherent defects such as transverse and longitudinal cracks, scabs or subsurface blowholes, which are not welded or eliminated after rolling and thus develop into surface cracks.
    (4) Uneven heating of the billet or uneven stress on the rolled piece leads to inconsistent elongation and width of each part, resulting in cracks under the action of stress.
    (5) Excessively fast heating or cooling rates cause intense concentration of thermal stress or structural stress, triggering the generation of cracks.
    (6) Excessive water spraying during rolling leads to an excessively low rolling temperature, which reduces the ductility of the steel plate and ultimately causes cracks.
    (7)The oxide scale is not removed in a timely manner during hot rolling and is pressed into the surface in subsequent rolling processes, forming defects.
  • 1.3 Solutions:
    (1) Strictly control the heating temperature and adopt inert gas to protect the furnace atmosphere.
    (2) Conduct surface cleaning prior to rolling, such as high-pressure water descaling with rotary nozzles, to ensure the oxide scale removal rate is ≥98%.
    (3) Leverage AI algorithms of modern technology to real-time monitor the geometric shape of steel plates and predict oxidation risks. Analyze historical data through machine learning models, and adjust heating parameters to avoid oxide scale accumulation.
    (4) AI algorithms can also be used to build a temperature control model. Combined with parameters such as the material characteristics of DIN XPM mold steel plates and billet dimensions, the model accurately calculates the optimal heating temperature, heating rate and cooling rate, and makes real-time dynamic adjustments. Collect billet temperature and rolled piece deformation data in real time and transmit it to the AI control system.

2. Loss of Dimensional Accuracy Control

  • 2.1 Problem: During the hot rolling process, the thickness, width and flatness of DIN XPM steel plates deviate from the tolerance range, resulting in issues such as uneven plate thickness, width deviation and warpage deformation. These problems often lead to difficulties in subsequent processing and increased production costs.
  • 2.2 Cause Analysis:
    (1) Roll wear and uneven surface abrasion lead to thickness fluctuation.
    (2) Temperature differences in the width direction cause edge warpage.
    (3) Unstable rolling force control, delayed response of the hydraulic system and fluctuation of the reduction amount.
    (4) Uneven temperature distribution in the heating furnace results in thermal stress concentration.
    (5) Mismatch between rolling speed and pressure leads to differential deformation.
    (6) Unstable thermal expansion coefficient, and temperature fluctuation of the billet during rolling causes uneven dimensional shrinkage.
    (7) Irrational design of rolling passes: the traditional process mostly relies on experience to set the reciprocating passes, leading to excessive temperature loss of the billet and compromising the final dimensional accuracy.
  • 2.3 Solutions:
    (1) Pre-set the rolling force according to the incoming material thickness, conduct real-time monitoring with an exit thickness gauge, and adjust the reduction amount within 0.1 seconds via AI algorithms.
    (2) Dynamically adjust the roll gap crown to compensate for the thermal expansion of rolls.
    (3) Establish a 3D thermal-mechanical coupling model to optimize the matching of rolling speed, reduction amount and roll speed for each pass, and control the thickness deviation within ±0.05 mm. Artificial intelligence, a modern technology, is adopted for real-time monitoring of temperature changes inside the heating furnace to optimize the heating process. Data analysis tools are used for fine adjustment of rolling parameters to ensure process stability.

3. Uneven Hardness

  • 3.1 Problem: The hardness difference at different positions of DIN XPM die steel plate exceeds 3HRC, with an obvious hardness gradient between the center and the edge.
  • 3.2 Cause Analysis:
    (1) The dendritic segregation in the as-cast structure is not fully broken during the hot rolling process.
    (2) Insufficient deformation and inadequate reduction at the central part result in incomplete recrystallization.
    (3) Uneven cooling, with the edge cooling faster than the center, creates a hardness difference. Excessively rapid water cooling induces a quenching effect, leading to a hard surface and a soft core; conversely, overly slow air cooling may cause coarse grain formation. The alloying elements of XPM steel (e.g., chromium, molybdenum) are temperature-sensitive, making the steel prone to the formation of stress concentration zones.
  • 3.3 Solutions:
    (1) Adopt controlled rolling with multiple passes and implement a three-stage process of high-temperature heavy deformation + medium-temperature controlled rolling + low-temperature finish rolling.
    (2) Control the cooling rate and set a cooling curve of 5–10 °C/min according to the steel plate thickness.
    (3) Conduct subsequent heat treatment to relieve residual stress.
    (4) Utilize AI to analyze metallurgical big data and optimize the cooling path, focus on the internal geometric structure of steel plates (e.g., grain distribution), and predict stress points through finite element simulation.

Conclusion

The hot rolling process of DIN XPM die steel plate is a sophisticated and precise systematic project. In addition to the core issues identified above, there are other challenges that require timely resolution. At Songshun Steel Works, we exercise stringent control over the details of every link in the hot rolling process of XPM die steel plate, achieving a dual improvement in production efficiency and product quality.

Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways
Or you can email directly to  sales@songshunsteel.com