Songshun Steel & TOP Steel Manufacturer Supplier in China

The Comprehensive Guide to Inconel 718

In the field of superalloys, Inconel 718 is definitely a “star player”. This alloy, renowned for its exceptional performance, is widely used in high-end sectors such as aerospace, petrochemicals, and energy, particularly excelling in high-temperature and corrosive environments. But do you truly understand Inconel 718 alloy steel? This article will comprehensively analyze it, including its equivalent grades, chemical composition, properties, applications, process specifications, and supply status, etc., allowing you to gain an in-depth understanding of this superalloy and striving to provide material support for your projects.

Inconel 718 Equivalent Grades

This alloy has different grade designations in various countries and regions, just like an “international citizen” holding “identity cards” from multiple countries.

  • Chinese standard GB/T 15007-2017: GB GH4169 (GH169) / ISC H41690
  • American standard ASTM B 637-2018: Inconel 718 / UNS N07718 / SAE XEV-1
  • American standard SAE AMS 5596 M-2017: AMS 5596
  • German standard EN 10269-2013: DIN NiCr19NbMo / DIN NiCr19Fe19Nb5Mo3 / W-Nr. 2.4668
  • French standards: NF ATG C1 / NF NC19FeNb

Inconel 718 Steel Chemical Composition

INCONEL 718 Chemical Element Composition Content (%)(ASTM B 637-2018 )
CSiMnPSCrNiCuMoTiNbBCoAlMore
≤0.08≤0.35≤0.35≤0.015≤0.01517.00-21.0050.00-55.00≤0.302.80-3.300.65-1.150.50-2.50≤0.006≤1.000.20-0.80Fe: balance; Nb+Ta:4.75~5.50

The exceptional performance of Inconel 718 is attributed to its meticulously formulated chemical composition, where each element acts like a “golden partner” to work synergistically. It contains a high nickel content of 50%-55%, which endows it with excellent oxidation resistance, high-temperature stability, and corrosion resistance. It also has a relatively high chromium content, serving as the “first line of defense” against corrosion. The optimal ratio of chromium to nickel not only ensures superior oxidation resistance, creep resistance, and sulfidation resistance but also provides a foundation for toughness. Molybdenum enhances the high-temperature strength and corrosion resistance of the alloy.

In addition, Inconel 718 material contains other elements that play important roles. It is the precise proportioning and interaction of these elements that give the material its unparalleled combination of properties, enabling it to perform excellently in various application scenarios.

Inconel 718 Alloy Steel Properties

  • Exceptionally high tensile strength and yield strength
  • Excellent corrosion resistance and oxidation resistance
  • Outstanding fatigue resistance and high-temperature stability
  • Relatively high hardness and wear resistance
  • Good creep resistance and fracture resistance
  • Superior weldability and machinability

Inconel 718 Application

Inconel 718 high temperature alloy steel has a wide range of applications, covering aerospace, oil and gas, nuclear energy, chemical industry, marine engineering, precision instruments and other key industries. It is usually used to manufacture aircraft engine turbine disks, blades, pipes, pump bodies, heat exchangers, measuring instrument components, implantable devices, nuclear reactor components, etc. Inconel 718 can work stably for a long time in various harsh environments, providing strong support for the development of high-end manufacturing industry.

Inconel 718 Process Specifications

To ensure Inconel 718, a high-nickel alloy, delivers optimal performance, two “magic processes”—forging and heat treatment—must be executed with meticulous care.

I. Forging Process

The forging temperature of the alloy is generally controlled between 980°C and 1150°C, with the final forging temperature being ≥950°C (to avoid δ phase precipitation). Within this temperature range, Inconel 718 exhibits good plasticity, facilitating forming. During forging, attention should be paid to uniform heating to prevent cracking caused by excessive temperature differences. After forging, water quenching or rapid air cooling should be performed to reduce internal stress, avoid grain coarsening, and prevent the precipitation of harmful phases. The purpose of this process is to improve the material’s internal structure and mechanical properties, making it more suitable for subsequent processing and application.

II.Heat Treatment Process

Typically, the heat treatment of Inconel 718 involves solution treatment and aging treatment. After heat treatment, not only are its strength and toughness further enhanced, but it can also meet performance requirements under various complex working conditions.

The solution treatment is conducted at a temperature of 950°C-1050°C, followed by water cooling after holding at this temperature for a certain period. The purpose is to fully dissolve the alloying elements into the matrix, forming a uniform solid solution.

Aging treatment is divided into two stages: in the first stage, the material is held at 720°C for 8 hours, then cooled to 620°C at a rate of 50°C per hour; in the second stage, it is held at 620°C for 8 hours followed by air cooling. Through aging treatment, strengthening phases can be precipitated, improving the alloy’s strength and hardness, and achieving an optimal balance between the alloy’s strength and toughness.

Conclusion

In summary, by gaining an understanding of this comprehensive guide to Inconel 718 supplied by Songshun, you will be able to select the most suitable and cost-effective material. In today’s era where pursuit of ultimate performance is paramount, Songshun is committed to providing you with high-performance Inconel 718 steel, offering high-quality material assurance for your projects and contributing to the greater success of your endeavors!

Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways
Or you can email directly to  sales@songshunsteel.com