Songshun Steel & TOP Steel Manufacturer Supplier in China

H13 Material Melting Process: EAF+LF+VD+ESR

As a core material in the mold manufacturing industry, the performance of H13 hot-work die steel (equivalent to DIN 1.2344, JIS SKD61 and GB 4Cr5MoSiV1) directly determines the service life of molds. Nevertheless, the outstanding properties of H13 material are not inherent; they stem from its complex and sophisticated melting process. So how is H13 steel produced? This article covers the complete melting workflow from EAF to ESR.

I. Why Is the Melting Process of H13 Material So Critical?


AISI H13 steel is a Cr-Mo-V alloy hot-work die steel. Featuring high strength, high toughness, excellent high-temperature resistance and superior thermal fatigue resistance, it is widely used for producing molds operating under high-temperature conditions.

At Songshun, all our H13 adopts a four-stage metallurgical process: EAF primary melting + LF refining + VD vacuum degassing + ESR electroslag remelting. The core objectives of this melting route include precise adjustment of alloy composition, deep removal of impurity gases, refinement of internal steel microstructure, and reduction of inclusion rating.

Furthermore, the H13 material melting process imposes stringent requirements on temperature, slag system, gas content and stirring rhythm. Only by strictly following the core principle — primary melting for impurity removal, refining for property adjustment, vacuum treatment for purification, and remelting for homogenization — can premium H13 die steel with low oxygen content, high cleanliness and stable performance be manufactured.

Ⅱ. H13 Material Core Melting Processes


The melting procedures of H13 are closely interconnected. Every stage is critical and directly governs the quality and performance of finished products. The whole process can be divided into the following key steps:

2.1 Raw Material Selection and Batching

Melting of H13 material commences with raw material selection. We select high-quality iron ore, scrap steel and alloying elements. The purity and proportion of these raw materials directly determine the ASTM H13 steel chemical composition and properties of the steel.

During batching, technicians test raw material purity via spectroscopic analysis in accordance with the standard compositional requirements of this steel grade, and precisely calculate the addition amount of each raw material to guarantee that the final chemical composition complies with specifications.

In addition, we clean residues and scale on the inner walls of electric arc furnaces and ladles before melting, and inspect equipment tightness to avoid contamination of molten steel by furnace impurities, creating a clean environment for subsequent melting operations.

2.2 EAF Primary Melting

Upon completion of batching, raw materials are fed into the electric arc furnace for primary melting. The electric arc furnace melts raw materials via high-temperature electric arcs and removes partial impurities simultaneously. Temperature control of the EAF is critical during this stage. We adjust furnace temperature, add lime for slag formation and introduce deoxidizers to rapidly melt raw materials, maintain the cleanliness of molten steel, preliminarily eliminate harmful impurities such as phosphorus and sulfur, and conduct alloying operations.

2.3 Secondary Refining (LF)

The molten steel after primary melting requires further refining. This stage serves as the core procedure for H13 material to optimize composition, conduct deep deoxidation and desulfurization, and improve steel cleanliness and homogeneity, addressing the problems of uneven composition and excessive impurities in primary molten steel.

At this stage, electric arc heating and bottom argon bubbling stirring are adopted to homogenize the temperature and composition of molten steel and remove impurities. Firstly, synthetic slag of the CaO-CaF₂-Al₂O₃ system is added, followed by aluminum granules and silicon carbide for diffusion deoxidation to form white slag for desulfurization. Under white slag conditions, impurities in steel are firmly captured into slag via slag-metal reactions, achieving ultra-clean steel grade.

Rapid sampling and spectroscopic analysis are carried out to precisely adjust the ratios of Cr, Mo and V, ensuring chemical composition falls within the ideal upper-middle range of standard tolerances (to guarantee hardenability and temper resistance). At the late stage of refining, silicon-calcium cored wire is fed deep into molten steel to transform large, angular Al₂O₃ inclusions into low-melting spherical calcium aluminates. Upon wire feeding completion, the bottom argon flow is adjusted to a low flow rate (without breaking the slag surface). The gas flotation effect enables fine inclusions to fully float up and be eliminated.

2.4 Vacuum Degassing (VD / RH)

Degassing treatment is implemented under vacuum conditions to remove hydrogen, oxygen, nitrogen and other dissolved gases from molten steel, further improving steel cleanliness and preventing porosity or cracking in subsequent service of H13/1.2344 steel.

Firstly, molten steel qualified after LF refining is held under vacuum with continuous bottom argon stirring for a certain duration to vigorously eliminate hydrogen (to avoid flakes), nitrogen and oxygen in molten steel, minimizing the total gas content.

Upon completion of vacuum treatment, low-flow gentle argon stirring is maintained for 5–8 minutes to homogenize molten steel temperature and composition, eliminate compositional fluctuations after vacuum processing and prevent re-gas absorption of molten steel.

2.5 Electroslag Remelting (ESR)

For high-end precision molds and applications requiring superior quality, the ESR H13 electroslag remelting process is adopted. This procedure can significantly refine steel grains, eliminate porosity and shrinkage cavities, and greatly enhance the toughness and thermal fatigue resistance of the steel.

First, qualified molten steel after vacuum treatment is cast into regular H13 consumable electrodes free of surface cracks, pores and oxidation defects. Afterwards, a quaternary slag system is used to precisely control melting current and voltage, enabling the consumable electrode to melt uniformly within the slag bath. The molten steel is filtered and purified when passing through the slag layer, effectively trapping residual micro-inclusions. The molten steel undergoes uniform directional solidification inside the crystallizer. The as-formed ESR ingot features dense microstructure, zero porosity and segregation, delivering mechanical properties far superior to conventionally melted H13 steel.

Ⅲ. FAQs on H13 Material Melting Process


Q1: Does the melting process of H13/1.2344/SKD61 steel affect heat treatment performance?
A: Absolutely. H13 material with low melting cleanliness and severe segregation can hardly achieve uniform microstructure and high toughness even with correct heat treatment parameters. Melting defines the steel’s “genetic properties”, while heat treatment serves as “acquired conditioning”.

Q2: Can VD vacuum degassing be omitted?
A: No. Omitting VD will lead to excessive hydrogen content. Flakes (hydrogen embrittlement cracks) are highly likely to form during subsequent heat treatment, triggering premature mold failure.

Q3: Is ESR mandatory for H13 melting?
A: It is not a must. For ordinary hot forging molds under non-extreme service conditions, the conventional EAF+LF+VD route can meet requirements. However, ESR is strongly recommended for high-end applications such as automotive die-casting molds, aerospace hot forging molds and large-section blocks. The service life can be increased by 2–3 times. In addition, it can drastically reduce inclusions, homogenize carbides and improve transverse toughness.

Conclusion


Every stage of the H13 melting process requires rigorous control, embodying the relentless pursuit of superior quality. Each procedure is designed to supply you with H13 steel products featuring outstanding performance and extended service life. Therefore, Songshun monitors every detail throughout the AISI H13 material melting process. We fully understand common melting defects and implement targeted prevention measures to manufacture optimal steel for you.

Whether you seek steel mill OEM cooperation, bulk steel stock procurement, or custom sourcing for end-use molds, feel free to contact us for high-quality H13 material solutions. Achieve doubled mold service life and drastically boosted production efficiency!

Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways
Or you can email directly to  sales@songshunsteel.com