As a high-end plastic mold steel, XPM steel meets the requirements for automotive lightweighting, precision manufacturing of 3C electronics, and high performance enhancement in aerospace, among other applications, by virtue of its excellent purity, high strength, high toughness and outstanding wear resistance, making it an ideal material for numerous fields that demand precision injection molds. But did you know? The robust performance of XPM die steel is inseparable from the precise refinement of the hot rolling process. This article will take an in-depth look at the core processes of the hot rolling technology applied to XPM mold steel supplied by Songshun.
The preparatory work prior to hot rolling directly determines the stability of the subsequent hot rolling process for XPM die steel, which consists of two core key steps:
(1) Billet Selection and Purification
DIN XPM steel imposes extremely high requirements on billet purity. We adopt high-purity ferroalloys and strictly control the precise proportioning of raw material components. Ingot castings produced by Electroslag Remelting (ESR) or Vacuum Induction Melting (VIM) are generally used as rolling billets. Such billets can effectively eliminate defects such as porosity, inclusions, segregation and shrinkage cavities in the as-cast structure, laying a solid foundation for the improvement of subsequent material performance. Meanwhile, the diameter/section size of the billet shall be accurately determined according to the finished product specifications, with a reasonable machining allowance reserved to avoid dimensional deviations caused by insufficient allowance during the subsequent rolling process.
(2) Surface Cleaning
Oxide scale, oil stains, cracks, rust, burrs and other defects on the ingot surface are thoroughly removed by means of mechanical grinding, shot blasting, sand blasting or pickling, so as to prevent the formation of blowhole defects during the hot rolling process. Meanwhile, ultrasonic flaw detection shall be conducted on the steel billet to ensure the absence of inherent defects such as internal cracks and porosity in the material.
Heating serves as the “prelude” to hot rolling, aiming to improve the plasticity of steel billets, reduce their deformation resistance, and meanwhile enable the full dissolution of carbides in the alloy, thereby creating favorable conditions for subsequent rolling. The heating process of DIN XPM die steel is divided into three stages, with millimeter-level precise temperature control to ensure uniform temperature throughout the steel billet and prevent internal stress concentration caused by temperature differences:
The first stage is the preheating phase: After the steel billet is charged into the furnace, it is slowly heated to a specified temperature for preheating, and the holding time is calculated based on the billet dimensions. The core of this stage is to homogenize the billet temperature and avoid thermal stress cracking induced by direct high-temperature heating. Especially for the high alloy content of XPM mold steel, slow preheating can effectively reduce the internal structural stress.
The second stage is the temperature rising phase: Upon completion of preheating, the temperature is increased at a rate of 120-180℃/h to 1100-1250℃. This temperature range is the optimal plasticity range for XPM mold steel, which ensures the full dissolution of carbides and prevents grain coarsening caused by excessively high temperatures.
The third stage is the soaking phase: The billet is held at 1100-1250℃ for 1.5-2.5 hours to ensure a completely uniform internal temperature, avoiding uneven deformation during rolling due to internal and external temperature differences. It is particularly important to use a heating furnace with a neutral or reducing atmosphere to minimize decarburization and oxidation on the billet surface.
A layer of oxide scale forms on the surface of steel billets during high-temperature heating. Therefore, at Songshun, the heated steel billets must undergo high-pressure water descaling before being fed into the rolling mill.
High-pressure water is adopted for the descaling of DIN XPM steel. The billet surface is rinsed comprehensively in all directions with fan-shaped water jets, which acts as a “water jet cutter” under multi-atmospheric pressure to strip off the oxide scale instantaneously. To ensure the descaling effect, the distance and angle between the water nozzles and the steel billet must be precisely adjusted to achieve full coverage without blind spots, with special attention devoted to the edge and corner parts of the billet.
Rolling is the core step for XPM die steel to form its final dimensions, microstructural and mechanical properties. The plastic deformation of steel billets is achieved through the synergistic operation of vertical rolling mills and horizontal rolling mills, and the entire process is divided into two stages: rough rolling and finish rolling.
(1) Rough Rolling Stage
The heated steel billets first undergo multi-pass rolling with heavy reduction on the roughing mill, with the rolling start temperature controlled at 1050–1150℃, a temperature range that endows the steel with excellent plasticity and low deformation resistance. Vertical rolling mills are first used for width reduction, followed by horizontal rolling mills for thickness reduction. The steel billets are rolled back and forth between the vertical and horizontal rolling mills for 3–5 passes, with the pass reduction controlled at 15%–25% in this stage. The objectives are to rapidly reduce the billet cross-sectional dimensions, break down the as-cast structure and refine grains, thereby laying a uniform microstructural foundation for subsequent finish rolling.
(2) Finish Rolling Stage
After the completion of rough rolling, the steel billets are directly fed into the finish rolling process while maintaining a specified surface temperature. Precision rolling with multiple passes and light reduction is applied to achieve the target thickness ultimately. Hot rolling of DIN XPM die steel adopts finish horizontal rolling mill stands and finish vertical rolling mill stands, with the steel billets being rolled back and forth between the two sets of mill stands for 5–7 passes and the pass reduction controlled at 8%–15%. Through the precise control of rolling force and speed, grain refinement is further realized, thickness uniformity is controlled, the dimensional accuracy and surface flatness of the finished products are guaranteed, and a pre-hardening effect is achieved.
After the completion of hot rolling, DIN XPM tool steel is subject to cooling treatment. Water cooling or oil cooling is generally adopted as the cooling method to control the material’s microstructure and achieve the desired mechanical properties.
After cooling, XPM die steel undergoes subsequent heat treatment to enhance its wear resistance and mechanical properties. Subsequent finishing processes are then carried out in accordance with customer requirements, including straightening, edge trimming, length cutting and surface polishing, to ensure dimensional accuracy and surface flatness of the product.
Finally, the material undergoes stringent quality inspection to verify compliance with relevant industry standards. Indispensable inspection procedures include hardness testing, microstructural analysis, ultrasonic flaw detection and surface roughness measurement—this constitutes a critical step in ensuring the quality of the steel.
In summary, every step in the hot rolling process of XPM die steel is indispensable. It is the synergistic effect of these steps that endows the material with excellent performance adaptable to numerous fields. At Songshun, we are able to precisely control the key considerations of each process in the hot rolling of XPM die steel plate. Going forward, we will continue to drive technological innovation and adopt more innovative hot rolling processes for XPM die material, providing customers with high-quality mold steel featuring more stable performance and a longer service life.