Songshun Steel & TOP Steel Manufacturer Supplier in China

Complete Manufacturing Process of Nickel Alloy 718

High-temperature alloy 718 steel has become a preferred material in a variety of manufacturing fields, including marine engineering, energy, and chemical engineering, thanks to its excellent performance. It can withstand temperatures exceeding 1,000 degrees Celsius, resist erosion from deep-sea pressures, and maintain stable mechanical properties. So, how is nickel alloy 718 manufactured? This article will fully reveal the manufacturing process of Inconel 718 steel, provided by Songshun.

I. Raw Materials

The rigorous screening of raw materials for Inconel 718 alloy steel is the first line of defense for quality. Usually, we will strictly select high-purity metal powders or bulk materials as raw materials, which must comply with relevant standards and specifications. Moreover, inspections such as spectral analysis, gas content detection and inclusion inspection are carried out to ensure that there are no impurities or defects. Only high-quality raw materials can lay a solid foundation for subsequent manufacturing processes.

II. Smelting Process

Smelting is the crucial first step in the manufacturing of nickel alloy 718, and it can be regarded as a “precise chemical reaction”. Typically, our traditional process adopts the double process of “Vacuum Induction Melting + Vacuum Arc Remelting” (VIM + VAR). For some high-end products, Electroslag Remelting (ESR) will be added to further improve purity, density and uniformity. Nowadays, the “triple process” (VIM + ESR + VAR) has become the mainstream choice for high-end Inconel 718 materials. The density of its ingots can reach 99.99%, which meets the strict requirements of key components such as aero-engine turbine disks.

In Vacuum Induction Melting (VIM), raw materials are mainly put into a graphite crucible in proportion and melted by electromagnetic induction heating. The vacuum environment can effectively remove gas impurities such as hydrogen and nitrogen, and prevent alloying elements from being oxidized. In Vacuum Arc Remelting (VAR), the ingot produced by VIM is mainly used as an electrode, which is remelted by arc discharge in a vacuum furnace, and the molten metal solidifies into a denser ingot in a water-cooled copper crucible. This step can refine grains and reduce segregation, which is the key to ensuring the uniformity of the material.

III. Forging/Casting/Rolling Processes

After smelting, although the ingot has high purity, its internal grains are coarse. Therefore, plastic processing methods such as forging or rolling are needed to “break” the grains, form the required shape and size, and improve the mechanical properties.

  • Forging/Casting: Hot forging is the core process for nickel alloy 718. The ingot is heated to 950-1200℃ (avoiding the brittle temperature zone) and subjected to pressure (upsetting + drawing out) by a hydraulic press or forging hammer to produce plastic deformation. Casting involves pouring molten alloy 718 steel into a suitable mold, which then solidifies into shape through continuous cooling. Common casting methods include vacuum projection and vacuum arc investment casting (VIM-VAR), etc. Whether during forging or casting, the degree of deformation must be strictly controlled to avoid affecting the quality due to excessive deformation. Both processes help to refine grains, eliminate as-cast defects, and improve the performance of the material.
  • Rolling: This process is suitable for producing nickel alloy 718 products such as plates, strips, or pipes. It mainly involves feeding the ingot into a rolling mill, where it is pressed into thin sheets or other shapes under the extrusion of upper and lower rolls to ensure uniform thickness of the material. It is worth noting that the “window period” for plastic processing of this steel is extremely short. A temperature fluctuation exceeding ±50℃ may lead to cracking. Therefore, real-time temperature measurement systems and intelligent temperature control equipment must be equipped, which is one of the reasons for its high processing cost.

IV. Heat Treatment Process

This process is a crucial step for the “customization” of nickel alloy 718’s properties. It mainly involves precisely controlling the heating temperature, holding time, and cooling rate to form uniform strengthening phases (such as γ” phase and γ’ phase) inside the alloy, thereby achieving a balance between strength and toughness.

  • Solution Treatment: The material is heated to a certain temperature, held for 1-2 hours, and then rapidly cooled. This allows the alloying elements to be fully dissolved into the matrix, with the aim of dissolving carbides and precipitated phases in the alloy, eliminating stress, and forming a uniform “solid solution”.
  • Aging Treatment: The material is first held at 720°C, then furnace-cooled to 620°C for further holding. This process promotes the uniform precipitation of γ” phase (Ni3Nb), which serves as the “main force” in enhancing the material’s strength and fatigue resistance.

V. Machining and Surface Treatment

Inconel 718 superalloy after heat treatment has high hardness and is a typical “difficult-to-machine material”. Its machining and surface treatment impose extremely high requirements on equipment and processes. Moreover, through these two processing techniques, the steel can meet the needs of more different application scenarios.

  • Machining: Processes such as turning, milling, drilling, and grinding are often used to precisely machine the shape and size of the alloy. It should be noted that ultra-fine grain cemented carbide tools or CBN (cubic boron nitride) tools need to be used, and the cutting speed, feed rate, and cooling method should be controlled. At the same time, special cooling oil (such as extreme pressure emulsion) is used to reduce frictional heat. For components with complex shapes (such as turbine blades), electrical discharge machining (EDM) or laser cutting is also adopted to ensure machining accuracy.
  • Surface Treatment: Different surface treatment processes are selected according to the application environment, including sandblasting, pickling, polishing, coating, nickel plating/aluminizing, etc. These processes further improve the surface quality and performance of nickel alloy 718, provide protection for harsh environments, and extend its service life.

Conclusion

To sum up, every link in the manufacturing process of nickel alloy 718 requires precise control. From raw materials to final products, its manufacturing process is not only a contest of technology, but also a test of the manufacturer’s experience and rigor. At Songshun, our nickel alloy 718 steel is strictly controlled from the smelting process, with precise regulation of the alloy composition ratio to ensure the purity and uniformity of the molten steel. The subsequent forging and rolling processes for nickel alloy 718 material are also continuously improved. Through multiple passes of high-temperature forging and precise rolling, the grain structure is refined, and the mechanical properties and dimensional accuracy of the material are enhanced, ensuring that each batch of steel can meet strict industry standards.

Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways
Or you can email directly to  sales@songshunsteel.com