AISI/ASTM H13 (equivalent to DIN 1.2344, JIS SKD61 and Chinese GB 4Cr5MoSiV1) is a chromium-molybdenum-vanadium hot work die steel that achieves an optimal balance among high-temperature strength, thermal fatigue resistance and toughness, and is widely used in various die manufacturing applications. For service conditions such as die-casting dies, hot forging dies and extrusion dies, the high-temperature mechanical properties of ASTM H13 hot work tool steel serve as the core metrics that truly determine die service life and production efficiency. The Cr-Mo-V alloy system retains stable strength, toughness and dimensional stability under repeated heating and cooling cycles. This paper elaborates on the high-temperature mechanical properties of ASTM H13 by temperature range.

I. High-Temperature Mechanical Properties of ASTM H13 Hot Work Tool Steel


The true test for hot work die steel lies at elevated temperatures. The alloy design of H13 steel targets retention of hardness and strength under continuous service temperatures around 540°C (1000°F), which is its “design service temperature”. Once exceeding this threshold, its properties degrade rapidly.

1. High-Temperature Tensile Properties: Strength vs. Temperature Curve

Tensile property is the primary indicator for evaluating the high-temperature load-bearing capacity of H13 hot work tool steel. Secondary hardening is achieved via strong carbide-forming elements including chromium, vanadium and molybdenum. Fine and dispersed alloy carbides precipitate during tempering, sustaining relatively high strength at high temperatures. The table below lists typical high-temperature tensile properties of AISI H13 steel after oil quenching plus double tempering. The steel is primarily austenitized at 1020–1050°C, oil quenched or vacuum gas quenched, followed by double tempering at 580–620°C (hardness: 48–52 HRC). Exact values vary depending on hardness grade and section size.

Test TemperatureTensile StrengthYield StrengthHardness (Cooled to Room Temperature)KV2 Charpy Impact EnergyElongation after Fracture, A (5D)
20°C≈1720 MPa≈1440 MPa≈50 HRC≈21 J≈13.2%
200°C≈1750 MPa≈1500 MPa≈49 HRC≈25 J≈14.5%
400°C≈1450 MPa≈1200 MPa≈48 HRC≈24 J≈15.0%
500°C≈1350 MPa≈1100 MPa≈47 HRC≈28 J≈17.0%
550°C≈1220 MPa≈980 MPa≈45 HRC≈32 J≈19.0%
600°C≈1050 MPa≈820 MPa≈42 HRC≈36 J≈22.0%
650°C≈780 MPa≈590 MPa≈36 HRC≈42 J≈28.0%
700°C≈480 MPa≈340 MPa≈26 HRC≈50 J≈40.0%

Actual values are affected by chemical composition, H13 tool steel ESR vs conventionally melted, forging ratio, specimen orientation, austenitizing temperature, number of tempering cycles, initial hardness, test strain rate and other factors.

2. High-Temperature Impact Toughness: Rising with Temperature

Impact toughness is an important indicator for evaluating the fracture resistance of ASTM H13 hot work tool steel under dynamic loads. Contrary to the trend of strength and hardness, the impact toughness of AISI H13 tool steel continuously increases as temperature rises. The Charpy impact energy is approximately 20–30 J at room temperature, rising to 30–45 J at 600°C and 42 J at 650°C.

This characteristic is critical for hot work dies:

  • Concerns about “brittleness” at room temperature do not apply under high-temperature service conditions
  • Dies possess higher toughness reserves at operating temperatures than those measured during factory inspection
  • High-temperature toughness plays a vital crack-arresting effect during the propagation of thermal fatigue cracks
  • Excellent thermal fatigue resistance under repeated heating and cooling cycles for hot forging dies

It should be noted that thermal shock is not equivalent to high-temperature impact toughness. Heat checking of ASTM H13 tool steel refers to thermal fatigue failure induced by repeated thermal expansion and contraction, which is a separate concept from impact toughness measured at a single temperature. The impact toughness of H13 is jointly affected by austenitizing temperature, grain size, inclusions, tempering regime, cooling rate and final hardness.

3. High-Temperature Hardness (Hot Hardness): The Most Intuitive Performance Indicator

Hot hardness is the core performance metric of hot work die steel, directly reflecting the material’s resistance to softening and wear at elevated temperatures. Variation in hardness of tempered ASTM H13 hot work tool steel with rising temperature:

  • ≤500°C: Hardness remains above 45 HRC with almost no noticeable softening
  • 500–550°C: Hardness decreases slowly with mild softening, maintaining 38–52 HRC
  • 550–600°C: Hardness drops markedly; each 50°C temperature rise reduces hardness by approximately 4–5 HRC
  • Above 600°C: Continuous softening occurs, reaching roughly 37 HRC at 650°C and about 30 HRC at 700°C

For aluminum alloy die casting, the hot hardness of H13 material is fully sufficient. However, for copper alloy die casting or applications under high heat load conditions, upgrading to ESR H13 or higher-grade hot work die steel is recommended.

II. FAQ on High-Temperature Mechanical Properties of ASTM H13 Hot Work Tool Steel


Q1: What are the differences in high-temperature properties between H13 and H11?

A1: AISI H13 has higher carbon and vanadium contents, delivering better hardness and wear resistance at 600°C than H11. H11 offers slightly higher toughness but inferior hot hardness. Select H13 for high-strength hot forging applications, while H11 is an option when high toughness is required.

Q2: How to improve the high-temperature mechanical properties of ASTM H13 hot work tool steel?

A2: Improve material cleanliness by adopting the Electro-Slag Remelting (ESR) process; optimize heat treatment procedures, especially tempering, to fully exploit the secondary hardening effect; apply surface strengthening treatments such as nitriding and nitrocarburizing; rationally design die structures to reduce stress concentration, and so on.

Q3: Does higher hardness of H13 always mean better wear resistance?

A3: This generally holds true at room temperature but not necessarily at elevated temperatures. Excessively high hardness (e.g., above 52 HRC) will markedly reduce toughness and thermal fatigue resistance, which may instead cause die failure due to premature heat checking. For high-temperature service conditions, 44–48 HRC is normally the optimal range for overall service life.

III. Conclusion


In addition to the properties discussed above, other key metrics for the high-temperature mechanical performance of ASTM H13 hot work tool steel include fracture toughness, creep and rupture strength, thermal fatigue resistance, and high-temperature elastic modulus. The core merit of this steel grade lies in achieving a balanced combination of these diverse properties.

Songshunsteel maintains a regular stock of AISI H13 / DIN 1.2344 / JIS SKD61. All products come with full mill test certificates and undergo quality inspection to ensure customers receive premium H13 steel.

Related Articles


Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways
Or you can email directly to  sales@songshunsteel.com