Songshun Steel & TOP Steel Manufacturer Supplier in China

AISI H13 Material Melting Process | Common Defects & Solutions

As a widely used high-quality hot work tool steel, AISI H13 boasts outstanding comprehensive properties including superior high-temperature resistance, fatigue resistance and high toughness. To guarantee the quality and performance of AISI H13 material, every detail of its melting process must be strictly controlled. This article elaborates on common defects occurring during the melting of this steel grade together with corresponding solutions, aiming to produce premium-quality materials.

I. AISI H13 Material Key Considerations for the Melting Process


The H13 material melting process uses scrap steel and alloy additives and consists of a series of metallurgical procedures: electric arc furnace primary melting → ladle refining (LF) → vacuum degassing (VD) → (electroslag remelting, ESR). This process directly determines its inclusion content, transverse toughness and service life of finished dies. Therefore, strict control over every detail in each melting stage is mandatory. Presented below are common defects arising in the melting process and their corresponding solutions.

① Raw Material Selection and Pretreatment Stage

Many steel mills overlook raw material screening, resulting in inherently excessive impurities and inhomogeneous composition in AISI H13 material, which constitute the primary inducements for cracking and inclusions in subsequent processes.

1.1 Key Technical Considerations

  • Strictly select furnace charge. Prioritize high-quality secondary-grade or superior scrap steel and high-purity pig iron. Inferior furnace materials with heavy rust, oil contamination or alloy impurities shall be prohibited.
  • Thoroughly remove residual steel and slag adhering to furnaces, ladles and central injection tubes in advance to prevent cross-contamination.
  • Rigorously control the initial content of harmful elements in raw materials to mitigate impurity risks at the source.

1.2 Defects & Countermeasures

  • Common Defects
    (1) Excessive impurities in raw materials lead to high inclusion rating and compositional segregation of steel products.
    (2) Entrapment of residual steel and slag causes inhomogeneous microstructure in finished products.
  • Solutions
    (1) Establish graded acceptance criteria for raw materials. Chemical composition testing is mandatory for every batch of incoming furnace charge.
    (2) Implement necessary pretreatment for raw materials simultaneously.
    (3) Perform complete purging and cleaning of furnaces and ladles prior to production.

② EAF Primary Melting Stage

Primary melting is the first core procedure for forming H13 steel and lays the foundation for smelting. Temperature, decarburization volume and tapping parameters directly determine the basic quality of molten steel. Its core tasks are dephosphorization and degassing, alongside controlling nitrogen pickup of liquid steel.

2.1 Key Technical Considerations

  • Implement slow and uniform temperature rise during the melting and heating phase to avoid uneven melting of furnace charge caused by rapid heating. Excessively high melting temperature may trigger vaporization of alloying elements, while overly low temperature leads to inhomogeneous molten bath and raises the risk of non-metallic inclusions.
  • Strictly control parameters in the oxidation stage to fully remove gases and impurities from molten steel.
  • Add preliminary deoxidizer synchronously when one-third of tapping is completed to pretreat molten steel in advance.
  • During EAF primary melting, once the nitrogen content in H13 molten steel exceeds 80 ppm, sharp titanium nitride inclusions will form, which directly impair polishability and fatigue life.
  • Maintain an inert or oxygen-reduced atmosphere inside the melting furnace to minimize metal oxidation and improve product quality to the maximum extent.

2.2 Defects & Countermeasures

  • Common Defects
    (1) Insufficient decarburization leading to carbide aggregation.
    (2) Incomplete dissolution of alloy elements caused by excessively low temperature.
    (3) Exposed molten steel for prolonged time, resulting in severe nitrogen pickup.
    (4) Excessive phosphorus content increasing cold shortness of steel.
  • Countermeasures
    (1) Continuously monitor furnace temperature and composition data in real time; adjust melting temperature dynamically to avoid tapping at low temperature.
    (2) Strictly implement intensive decarburization process to meet decarburization target and purify molten steel matrix.
    (3) Adopt foaming slag submerged arc operation to shorten arc exposure time and reduce nitrogen absorption via atmospheric ionization.
    (4) Apply full-process slag blocking during tapping; strictly prevent slag carryover into ladle to lower the risk of slag inclusion defects.

③ LF Refining Stage

This process is critical for optimizing the alloy composition of AISI H13 material, implementing efficient deoxidation and slag formation, reducing inclusions, and homogenizing microstructure. It directly determines the toughness and stability of the steel.

3.1 Key Technical Considerations

  • Adopt gradient diffusion deoxidation process; conduct staged temperature-controlled deoxidation and cooling with 7–10 minutes holding time for each stage.
  • Add deoxidizers in batches.
  • Implement full-process argon stirring to ensure sufficient contact between molten steel and slag. The total slag volume shall be controlled at approximately 30 kg/t. Prioritize fine-tuning core alloy elements including Cr, Mo and V in the early stage to make composition conform to AISI H13 specifications.
  • Rigorously control refining duration to achieve thorough purification of molten steel.

3.2 Defects & Countermeasures

  • Common Defects
    (1) Incomplete deoxidation leading to excessive alumina inclusions.
    (2) Uneven stirring resulting in composition segregation.
    (3) Deviated alloy ratio causing substandard hardness and toughness of steel.

  • Countermeasures

    (1) Adopt segmented precise deoxidation mode to avoid uneven deoxidation caused by one-time deoxidation. Deploy filters to further remove inclusions from molten steel.
    (2) Maintain constant-flow argon stirring throughout the process to eliminate composition dead zones.
    (3) Take samples for re-inspection of composition after refining; conduct real-time monitoring and precise fine-tuning of alloy ratios to ensure all parameters fully comply with AISI H13 standards.
    (4) Replace refining slag regularly to guarantee slagging and impurity removal performance.

④ Vacuum Degassing Stage

This process serves to degas and purify molten steel to eliminate shrinkage and blowholes. Excessive hydrogen and oxygen contents in AISI H13 steel are the primary causes of blowholes, internal shrinkage and heat treatment cracking in finished products; therefore, the VD degassing stage is indispensable.

4.1 Key Technical Considerations

  • Strictly control vacuum level, maintain an ultimate vacuum state and ensure sufficient vacuum holding time.
  • Adopt high-flow intense argon stirring process to facilitate the floating and separation of dissolved gases and inclusions from molten steel.
  • Thoroughly remove hydrogen and oxygen in steel, lower the rating of oxide inclusions and improve the cleanliness of molten steel.
  • Prevent air backflow during degassing to avoid reoxidation of molten steel.

4.2 Defects & Countermeasures

  • Common Defects
    (1) Inadequate vacuum degassing leading to internal blowholes and shrinkage in steel.
    (2) Excessive residual inclusions shortening die service life.
    (3) Hydrogen embrittlement and flakes induced by excessive hydrogen content in steel.

  • Countermeasures

    (1) Monitor vacuum equipment parameters in real time to ensure stable and qualified ultimate vacuum level. Avoid inadequate short-cycle degassing and strengthen vacuum degassing procedures.
    (2) Optimize argon stirring parameters to enhance mass transfer and separation of inclusions. Maintain sufficient standing time after degassing for full flotation and removal of fine residual inclusions.
    (3) Implement rigorous VD vacuum degassing, and perform hydrogen diffusion holding treatment at specified temperature during the ingot heating stage.

⑤ Electroslag Remelting (ESR) Stage

This stage optimizes microstructure and improves steel homogeneity. Therefore, ESR H13 steel electroslag remelting precautions are critical, which constitute the key to distinguishing standard-grade material from premium-grade material.

5.1 Key Technical Considerations

  • Machine primary ingots into standard electrodes; strictly ensure electrode surfaces are free of cracks and contaminants.
  • Precisely control remelting current, voltage and cooling rate to achieve uniform layer-by-layer solidification of the ingot.
  • Stabilize the temperature field throughout remelting to prevent local overheating or excessive rapid cooling, and avoid precipitation and aggregation of carbides along grain boundaries.

5.2 Defects & Countermeasures

  • Common Defects
    (1) Unstable remelting parameters resulting in inhomogeneous microstructure and severe carbide segregation.
    (2) Improper cooling inducing internal microcracks in the ingot.

  • Countermeasures

    (1) Deploy automatic temperature-controlled remelting equipment to maintain constant parameters during the whole process.
    (2) Adopt uniform cooling after remelting to avoid drastic temperature fluctuations.
    (3) Significantly reduce harmful impurities via electroslag remelting. Control sulfur content within the range of 0.005%–0.008% to produce high-purity premium AISI H13 material.

II. FAQs on Melting Precautions for AISI H13 Material


Q1: What points should be noted in the deoxidation stage?

A1: Aluminum and Si–Ca alloys are commonly adopted for final deoxidation. The acid-soluble aluminum (Als) content shall be controlled within a reasonable range. Excessive aluminum addition must be avoided, as surplus Al will form clustered brittle Al₂O₃ inclusions, which impair fatigue life and exhibit poor deformability. Calcium treatment is recommended to transform strip-shaped Al₂O₃ into low-melting spherical calcium aluminates (CaO–Al₂O₃), thereby improving machinability, polishability and toughness.

Q2: What are the critical control targets during LF refining?

A2: Key controls include slag system and basicity, deep deoxidation, desulfurization timing, and staged bottom argon blowing.

Q3: What precautions are required for primary melting (EAF/BOF)?

A3: It is necessary to prevent over-oxidation of molten steel, strictly prohibit rephosphorization caused by slag carryover, and utilize low-titanium raw materials together with low-titanium ladles.

Conclusion


Every stage of the melting process for AISI H13 material, from raw material selection, EAF primary melting, LF refining, VD vacuum degassing to electroslag remelting, requires stringent control. At Songshun, we guarantee the process quality of ASTM H13 material and commit to manufacturing premium die steel that meets international inclusion rating and testing standards.

Whether you are steel stockists, end-user mold manufacturers or purchasers from steel mills in need of high-quality H13 steel, you may refer to our contacts anytime.

Songshun Steel-Logo

Dongguan Songshun Mould Steel Co., Ltd.

Welcome to contact us at any time through the following ways
Or you can email directly to  sales@songshunsteel.com